Frequently Asked Questions
Soft resin use common problems and solutions
1, the product is too strong or too crisp
Formation reason: curing too fast
Solution: reduce the proportion of curing agent and accelerator
2. Products are too soft and sticky
Formation reason: curing too slow
Solution: increase the proportion of curing agent and accelerator
3. Burst after assembly
Formation reason: powder added too much or uneven mixing.
Solution: reduce the proportion of stone powder, stir thoroughly
Cause of formation: The bubbles do not drain clean
Solution: increase the time of evacuation or extend the gelation time
Formation reason: curing too fast
Solution: Adjust the proportion of curing agent and accelerator
Problem not solved? Online submission help

Huizhou GoodUPR Compites Ltd.
Address:F-22-3 Honghai base, Yonghu Huiyang, Huizhou
TEL : +86 0752-3588066
FAX : +86 0752-3588065
E-Mail : export@goodupr.com