1、Products are too hard or brittle

Formation reasons:Curing fast.

Solution:Reduce the proportion of curing agent and accelerator.

 

2、The product is too soft and sticky

Formation reasons:Curing is too slow.

Solution:Increase the proportion of curing agent and accelerator.

 

3、Burst after assembly

Formation reasons:Add too much powder or mix unevenly.

Solution:Reduce the proportion of stone powder and mix well.

 

Formation reasons:Bubbles didn't clear out.

Solution:Increase the pumping time or prolong the gelation time.

 

Formation reasons:Curing fast.

Solution:Adjust the proportion of curing agent and accelerator.

 